Residual stress profiles in veneering ceramic on Y-TZP, alumina and ZTA frameworks: Measurement by hole-drilling
Fukushima, K. A.; Sadoun, M. J.; Cesar, P. F. et al.
2014In Dental Materials, 30 (2), p. 105-111
Peer Reviewed verified by ORBi
 

Files


Full Text
Fukushima2013.doc
Author postprint (194.05 kB)
Request a copy

All documents in ORBi are protected by a user license.

Send to



Details



Keywords :
Alumina; Chipping; Hole-drilling; Residual stress; Veneering ceramic; Zirconia; Zirconia toughened alumina
Abstract :
[en] OBJECTIVES: The residual stress profile developed within the veneering ceramic during the manufacturing process is an important predicting factor in chipping failures, which constitute a well-known problem with yttria-tetragonal-zirconia polycrystal (Y-TZP) based restorations. The objectives of this study are to measure and to compare the residual stress profile in the veneering ceramic layered on three different polycrystalline ceramic framework materials: Y-TZP, alumina polycrystal (AL) and zirconia toughened alumina (ZTA). METHODS: The stress profile was measured with the hole-drilling method in bilayered disk samples of 19mm diameter with a 0.7mm thick Y-TZP, AL or ZTA framework and a 1.5mm thick layer of the corresponding veneering ceramic. RESULTS: The AL samples exhibited increasing compressive stresses with depth, while compressive stresses switching into interior tensile stresses were measured in Y-TZP samples. ZTA samples exhibited compressive stress at the ceramic surface, decreasing with depth up to 0.6mm from the surface, and then becoming compressive again near the framework. SIGNIFICANCE: Y-TZP samples exhibited a less favorable stress profile than those of AL and ZTA samples. Results support the hypothesis of the occurrence of structural changes within the Y-TZP surface in contact with the veneering ceramic to explain the presence of tensile stresses. Even if the presence of Y-TZP in the alumina matrix seems to negatively affect the residual stress profiles in ZTA samples in comparison with AL samples, the registered profiles remain positive in terms of veneer fracture resistance.
Research center :
d‐BRU - Dental Biomaterials Research Unit - ULiège [BE]
Disciplines :
Materials science & engineering
Dentistry & oral medicine
Author, co-author :
Fukushima, K. A.
Sadoun, M. J.
Cesar, P. F.
MAINJOT, Amélie  ;  Centre Hospitalier Universitaire de Liège - CHU > Institut de dentisterie - prothèse fixée
Language :
English
Title :
Residual stress profiles in veneering ceramic on Y-TZP, alumina and ZTA frameworks: Measurement by hole-drilling
Publication date :
February 2014
Journal title :
Dental Materials
ISSN :
0109-5641
eISSN :
1879-0097
Publisher :
Elsevier, Netherlands
Volume :
30
Issue :
2
Pages :
105-111
Peer reviewed :
Peer Reviewed verified by ORBi
Commentary :
Copyright (c) 2013 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Available on ORBi :
since 08 January 2014

Statistics


Number of views
74 (2 by ULiège)
Number of downloads
2 (1 by ULiège)

Scopus citations®
 
23
Scopus citations®
without self-citations
18
OpenCitations
 
23

Bibliography


Similar publications



Contact ORBi