Karevan, Yousef ✱; Université de Liège - ULiège > Dental biomaterials research unit (d-BRU)
Eldafrawy, Maher ✱; Université de Liège - ULiège > Département des sciences dentaires > Biomatériaux dentaires
Herman, Raphaël ; Université de Liège - ULiège > Département des sciences dentaires > Biomatériaux dentaires ; Université de Liège - ULiège > Dental biomaterials research unit (d-BRU)
Sanchez, Christelle ; Université de Liège - ULiège > Département des sciences dentaires > Biomatériaux dentaires ; Centre Hospitalier Universitaire de Liège - CHU > > Service prothèse fixée
Sadoun, Michael
Mainjot, Amélie ; Université de Liège - ULiège > Département des sciences dentaires > Biomatériaux dentaires ; Université de Liège - ULiège > Dental biomaterials research unit (d-BRU) ; Centre Hospitalier Universitaire de Liège - CHU > > Service prothèse fixée
✱ These authors have contributed equally to this work.
Language :
English
Title :
Do all ceramic and composite CAD-CAM materials exhibit equal bonding properties to implant Ti-base materials? An Interfacial Fracture Toughness Study
Kapos, T., Evans, C., CAD/CAM technology for implant abutments, crowns, and superstructures. Int J Oral Maxillofac Implants 29 (2014), 117–136, 10.11607/jomi.2014suppl.g2.3.
Makhija, S.K., Lawson, N.C., Gilbert, G.H., Litaker, M.S., McClelland, J.A., Louis, D.R., et al. Dentist material selection for single-unit crowns: findings from the National Dental Practice-Based Research Network. J Dent 55 (2016), 40–47, 10.1016/j.jdent.2016.09.010.
Lambert, H., Durand, J.-C., Jacquot, B., Fages, M., Dental biomaterials for chairside CAD/CAM: state of the art. J Adv Prosthodont, 9, 2017, 486, 10.4047/jap.2017.9.6.486.
Ahmed, K.E., We're going digital: the current state of CAD/CAM dentistry in prosthodontics. Prim Dent J 7 (2018), 30–35, 10.1177/205016841800700205.
Belli, R., Petschelt, A., Hofner, B., Hajtó, J., Scherrer, S.S., Lohbauer, U., Fracture rates and lifetime estimations of CAD/CAM all-ceramic restorations. J Dent Res 95 (2016), 67–73, 10.1177/0022034515608187.
Rosentritt, M., Hahnel, S., Engelhardt, F., Behr, M., Preis, V., In vitro performance and fracture resistance of CAD/CAM-fabricated implant supported molar crowns. Clin Oral Invest 21 (2017), 1213–1219, 10.1007/s00784-016-1898-9.
Carames, J., Tovar Suinaga, L., Yu, Y.C.P., Pérez, A., Kang, M., Clinical advantages and limitations of monolithic zirconia restorations full arch implant supported reconstruction: case series. Int J Dent 2015 (2015), 1–7, 10.1155/2015/392496.
Sadid-Zadeh, R., Liu, P.-R., Aponte-Wesson, R., O'Neal, S.J., Maxillary cement retained implant supported monolithic zirconia prosthesis in a full mouth rehabilitation: a clinical report. J Adv Prosthodont, 5, 2013, 209, 10.4047/jap.2013.5.2.209.
Coldea, A., Fischer, J., Swain, M.V., Thiel, N., Damage tolerance of indirect restorative materials (including PICN) after simulated bur adjustments. Dent Mater 31 (2015), 684–694, 10.1016/j.dental.2015.03.007.
Lebon, N., Tapie, L., Vennat, E., Mawussi, B., Influence of CAD/CAM tool and material on tool wear and roughness of dental prostheses after milling. J Prosthet Dent 114 (2015), 236–247, 10.1016/j.prosdent.2014.12.021.
Mainjot, A.K., Dupont, N.M., Oudkerk, J.C., Dewael, T.Y., Sadoun, M.J., From artisanal to CAD-CAM blocks: state of the art of indirect composites. J Dent Res 95 (2016), 487–495, 10.1177/0022034516634286.
Mainjot, A.K.J., The One step‐No prep technique: a straightforward and minimally invasive approach for full‐mouth rehabilitation of worn dentition using polymer‐infiltrated ceramic network (PICN) CAD‐CAM prostheses. J Esthet Restor Dent 32 (2020), 141–149, 10.1111/jerd.12432.
Zaghloul, H., Elkassas, D.W., Haridy, M.F., Effect of incorporation of silane in the bonding agent on the repair potential of machinable esthetic blocks. Eur J Dent 08 (2014), 044–052, 10.4103/1305-7456.126240.
Mainjot, A., Recent advances in composite CAD/CAM blocks. Int J Esthet Dent 11 (2016), 275–280.
Nguyen, J.F., Ruse, D., Phan, A.C., Sadoun, M.J., High-temperature-pressure polymerized resin-infiltrated ceramic networks. J Dent Res 93 (2014), 62–67, 10.1177/0022034513511972.
Sailer, I., Karasan, D., Todorovic, A., Ligoutsikou, M., Pjetursson, B.E., Prosthetic failures in dental implant therapy. Periodontol 2000 88 (2022), 130–144, 10.1111/prd.12416.
Chantler, J.G.M., Evans, C.D.J., Zitzmann, N.U., Derksen, W., Clinical performance of single implant prostheses restored using titanium base abutments: A systematic review and meta‐analysis. Clin Oral Implants Res 34 (2023), 64–85, 10.1111/clr.14128.
Lemos, C.A.A., Verri, F.R., De Luna Gomes, J.M., Santiago Junior, J.F., Miyashita, E., Mendonça, G., et al. Survival and prosthetic complications of monolithic ceramic implant-supported single crowns and fixed partial dentures: a systematic review with meta-analysis. J Prosthet Dent, 2022, S0022391322007363, 10.1016/j.prosdent.2022.11.013.
Derksen, W., Tahmaseb, A., Wismeijer, D., Randomized Clinical Trial comparing clinical adjustment times of CAD/CAM screw‐retained posterior crowns on ti‐base abutments created with digital or conventional impressions. One‐year follow‐up. Clin Oral Implants Res 32 (2021), 962–970, 10.1111/clr.13790.
Koenig, V., Wulfman, C., Bekaert, S., Dupont, N., Le Goff, S., Eldafrawy, M., et al. Clinical behavior of second-generation zirconia monolithic posterior restorations: two-year results of a prospective study with Ex vivo analyses including patients with clinical signs of bruxism. J Dent, 91, 2019, 103229, 10.1016/j.jdent.2019.103229.
Lambert, F., Eldafrawy, M., Bekaert, S., Mainjot, A., One-tooth one-time (1T1T), immediate loading of posterior single implants with the final crown: 2-year results of a case series. Int J Oral Implant 13 (2020), 369–383.
Pitta, J., Burkhardt, F., Mekki, M., Fehmer, V., Mojon, P., Sailer, I., Effect of airborne-particle abrasion of a titanium base abutment on the stability of the bonded interface and retention forces of crowns after artificial aging. J Prosthet Dent 126 (2021), 214–221, 10.1016/j.prosdent.2020.06.013.
Krejci, I., Daher, R., Stress distribution difference between Lava Ultimate full crowns and IPS e.max CAD full crowns on a natural tooth and on tooth-shaped implant abutments. Odontology 105 (2017), 254–256, 10.1007/s10266-016-0276-z.
Matinlinna, J.P., Processing and bonding of dental ceramics. Non-Met. Biomater. Tooth Repair Replace, 2013, Elsevier, 129–160, 10.1533/9780857096432.2.129.
Matinlinna, J.P., Lung, C.Y.K., Tsoi, J.K.H., Silane adhesion mechanism in dental applications and surface treatments: a review. Dent Mater 34 (2018), 13–28, 10.1016/j.dental.2017.09.002.
Serichetaphongse, P., Chitsutheesiri, S., Chengprapakorn, W., Comparison of the shear bond strength of composite resins with zirconia and titanium using different resin cements. J Prosthodont Res 66 (2022), 109–116, 10.2186/jpr.JPR_D_20_00299.
Maravić, T., Mazzitelli, C., Mancuso, E., Del Bianco, F., Josić, U., Cadenaro, M., et al. Resin composite cements: current status and a novel classification proposal. J Esthet Restor Dent 35 (2023), 1085–1097, 10.1111/jerd.13036.
Yoshihara, K., Nagaoka, N., Sonoda, A., Maruo, Y., Makita, Y., Okihara, T., et al. Effectiveness and stability of silane coupling agent incorporated in ‘universal’ adhesives. Dent Mater 32 (2016), 1218–1225, 10.1016/j.dental.2016.07.002.
Yao, C., Yu, J., Wang, Y., Tang, C., Huang, C., Acidic pH weakens the bonding effectiveness of silane contained in universal adhesives. Dent Mater 34 (2018), 809–818, 10.1016/j.dental.2018.02.004.
Yoshihara, K., Nagaoka, N., Maruo, Y., Nishigawa, G., Yoshida, Y., Van Meerbeek, B., Silane-coupling effect of a silane-containing self-adhesive composite cement. Dent Mater 36 (2020), 914–926, 10.1016/j.dental.2020.04.014.
Dimitriadi, M., Petropoulou, A., Vakou, D., Zinelis, S., Eliades, G., In vitro evaluation of a silane containing self-adhesive resin luting agent. Dent Mater 39 (2023), 181–191, 10.1016/j.dental.2022.12.007.
Eldafrawy, M., Bekaert, S., Nguyen, J.-F., Sadoun, M., Mainjot, A., Bonding properties of third-generation zirconia CAD-CAM blocks for monolithic restorations to composite and resin-modified glass-ionomer cements. J Prosthodont Res 66 (2022), 466–475, 10.2186/jpr.JPR_D_21_00044.
Zahoui, A., Bergamo, E., Marun, M., Silva, K., Coelho, P., Bonfante, E., Cementation protocol for bonding zirconia crowns to titanium base CAD/CAM abutments. Int J Prosthodont 33 (2020), 527–535, 10.11607/ijp.6696.
Hansen, N.A., Wille, S., Kern, M., Effect of reduced airborne-particle abrasion pressure on the retention of zirconia copings resin bonded to titanium abutments. J Prosthet Dent 124 (2020), 60–67, 10.1016/j.prosdent.2019.07.001.
Lang, R., Hiller, K.-A., Kienböck, L., Friedl, K., Friedl, K.-H., Influence of autoclave sterilization on bond strength between zirconia frameworks and Ti-base abutments using different resin cements. 617.e1-617.e6 J Prosthet Dent, 127, 2022, 10.1016/j.prosdent.2022.01.028.
Wiedenmann, F., Liebermann, A., Spintzyk, S., Eichberger, M., Stawarczyk, B., Influence of different cleaning procedures on tensile bond strength between zirconia abutment and titanium base. Int J Oral Maxillofac Implants 34 (2019), 1318–1327, 10.11607/jomi.7638.
T. P. Bergamo, E., Zahoui, A., Luri Amorin Ikejiri, L., Marun, M., Peixoto Da Silva, K., G. Coelho, P., et al. Retention of zirconia crowns to Ti-base abutments: effect of luting protocol, abutment treatment and autoclave sterilization. J Prosthodont Res 65 (2021), 171–175, 10.2186/jpr.JPOR_2019_537.
Mehl, C., Zhang, Q., Lehmann, F., Kern, M., Retention of zirconia on titanium in two-piece abutments with self-adhesive resin cements. J Prosthet Dent 120 (2018), 214–219, 10.1016/j.prosdent.2017.11.020.
Arce, C., Lawson, N., Liu, P.-R., Lin, C., Givan, D., Retentive force of zirconia implant crowns on titanium bases following different surface treatments. Int J Oral Maxillofac Implants 33 (2018), 530–535, 10.11607/jomi.5915.
Burkhardt, F., Pitta, J., Fehmer, V., Mojon, P., Sailer, I., Retention forces of monolithic CAD/CAM crowns adhesively cemented to titanium base abutments—effect of saliva contamination followed by cleaning of the titanium bond surface. Materials, 14, 2021, 3375, 10.3390/ma14123375.
Nouh, I., Kern, M., Sabet, A.E., Aboelfadl, A.K., Hamdy, A.M., Chaar, M.S., Mechanical behavior of posterior all‐ceramic hybrid‐abutment‐crowns versus hybrid‐abutments with separate crowns—a laboratory study. Clin Oral Implants Res 30 (2019), 90–98, 10.1111/clr.13395.
Burkhardt, F., Sailer, I., Fehmer, V., Mojon, P., Pitta, J., Retention and marginal integrity of CAD/CAM fabricated crowns adhesively cemented to titanium base abutments—influence of bonding system and restorative material. Int J Prosthodont, 36, 2023, 10.11607/ijp.7576.
Rödiger, M., Kloß, J., Gersdorff, N., Bürgers, R., Rinke, S., Removal forces of adhesively and self-adhesively luted implant-supported zirconia copings depend on abutment geometry. J Mech Behav Biomed Mater 87 (2018), 119–123, 10.1016/j.jmbbm.2018.07.028.
Rödiger, M., Rinke, S., Ehret-Kleinau, F., Pohlmeyer, F., Lange, K., Bürgers, R., et al. Evaluation of removal forces of implant-supported zirconia copings depending on abutment geometry, luting agent and cleaning method during re-cementation. J Adv Prosthodont, 6, 2014, 233, 10.4047/jap.2014.6.3.233.
De Jager, N., Pallav, P., Feilzer, A.J., The influence of design parameters on the FEA-determined stress distribution in CAD–CAM produced all-ceramic dental crowns. Dent Mater 21 (2005), 242–251, 10.1016/j.dental.2004.03.013.
Karaokutan, I., Ozel, G.S., Effect of surface treatment and luting agent type on shear bond strength of titanium to ceramic materials. J Adv Prosthodont, 14, 2022, 78, 10.4047/jap.2022.14.2.78.
Guilherme, N., Wadhwani, C., Zheng, C., Chung, K.-H., Effect of surface treatments on titanium alloy bonding to lithium disilicate glass-ceramics. J Prosthet Dent 116 (2016), 797–802, 10.1016/j.prosdent.2016.04.023.
Amornwichitwech, L., Palanuwech, M., Shear bond strength of lithium disilicate bonded with various surface-treated titanium. Int J Dent 2022 (2022), 1–11, 10.1155/2022/4406703.
Scherrer, S.S., Cesar, P.F., Swain, M.V., Direct comparison of the bond strength results of the different test methods: a critical literature review. Dent Mater 26 (2010), e78–e93, 10.1016/j.dental.2009.12.002.
Van Meerbeek, B., Peumans, M., Poitevin, A., Mine, A., Van Ende, A., Neves, A., et al. Relationship between bond-strength tests and clinical outcomes. Dent Mater 26 (2010), e100–e121, 10.1016/j.dental.2009.11.148.
Armstrong, S., Geraldeli, S., Maia, R., Raposo, L.H.A., Soares, C.J., Yamagawa, J., Adhesion to tooth structure: a critical review of “micro” bond strength test methods. Dent Mater 26 (2010), e50–e62, 10.1016/j.dental.2009.11.155.
Soderholm, K.-J., Review of the fracture toughness approach. Dent Mater 26 (2010), e63–e77, 10.1016/j.dental.2009.11.151.
De Munck, J., Luehrs, A.-K., Poitevin, A., Van Ende, A., Van Meerbeek, B., Fracture toughness versus micro-tensile bond strength testing of adhesive–dentin interfaces. Dent Mater 29 (2013), 635–644, 10.1016/j.dental.2013.03.010.
Pongprueksa, P., De Munck, J., Karunratanakul, K., Barreto, B.C., Van Ende, A., Senawongse, P., et al. Dentin bonding testing using a mini-interfacial fracture toughness approach. J Dent Res 95 (2016), 327–333, 10.1177/0022034515618960.
Cesar, P.F., Della Bona, A., Scherrer, S.S., Tholey, M., Van Noort, R., Vichi, A., et al. ADM guidance—ceramics: fracture toughness testing and method selection. Dent Mater 33 (2017), 575–584, 10.1016/j.dental.2017.03.006.
Ruse, N.D., Troczynski, T., MacEntee, M.I., Feduik, D., Novel fracture toughness test using a notchless triangular prism (NTP) specimen. J Biomed Mater Res 31 (1996), 457–463, 10.1002/(SICI)1097-4636(199608)31:4<457::AID-JBM4>3.0.CO;2-K.
Ilie, N., Ruse, N.D., Shear bond strength vs interfacial fracture toughness — adherence to CAD/CAM blocks. Dent Mater 35 (2019), 1769–1775, 10.1016/j.dental.2019.10.003.
De Munck, J., Van Landuyt, K., Peumans, M., Poitevin, A., Lambrechts, P., Braem, M., et al. A critical review of the durability of adhesion to tooth tissue: methods and results. J Dent Res 84 (2005), 118–132, 10.1177/154405910508400204.
Armstrong, S., Breschi, L., Özcan, M., Pfefferkorn, F., Ferrari, M., Van Meerbeek, B., Academy of dental materials guidance on in vitro testing of dental composite bonding effectiveness to dentin/enamel using micro-tensile bond strength (μTBS) approach. Dent Mater 33 (2017), 133–143, 10.1016/j.dental.2016.11.015.
Munz, D., Fett, T., Ceramics: mechanical properties, failure behaviour, materials selection. 2001, Springer-Verlag, Berlin Heidelberg.
Zorzin, J., Beck, S., Belli, R., Petschelt, A., Boccaccini, A.R., Lohbauer, U., Adhesion and interfacial characterization of biomimetically texturized lithium disilicate. Int J Adhes Adhes 91 (2019), 131–141, 10.1016/j.ijadhadh.2019.03.012.
Bütikofer, L., Stawarczyk, B., Roos, M., Two regression methods for estimation of a two-parameter Weibull distribution for reliability of dental materials. Dent Mater 31 (2015), e33–e50, 10.1016/j.dental.2014.11.014.
Fathi, A., Hashemi, S., Tabatabaei, S., Mosharraf, R., Atash, R., Adhesion to zirconia: an umbrella review. Int J Adhes Adhes, 122, 2023, 103322, 10.1016/j.ijadhadh.2023.103322.
Mine, A., Kabetani, T., Kawaguchi-Uemura, A., Higashi, M., Tajiri, Y., Hagino, R., et al. Effectiveness of current adhesive systems when bonding to CAD/CAM indirect resin materials: a review of 32 publications. Jpn Dent Sci Rev 55 (2019), 41–50, 10.1016/j.jdsr.2018.10.001.
Yoshihara, K., Nagaoka, N., Maruo, Y., Nishigawa, G., Irie, M., Yoshida, Y., et al. Sandblasting may damage the surface of composite CAD–CAM blocks. Dent Mater 33 (2017), e124–e135, 10.1016/j.dental.2016.12.003.
Eldafrawy, M., Greimers, L., Bekaert, S., Gailly, P., Lenaerts, C., Nguyen, J.-F., et al. Silane influence on bonding to CAD-CAM composites: an interfacial fracture toughness study. Dent Mater 35 (2019), 1279–1290, 10.1016/j.dental.2019.05.019.
Eldafrawy, M., Ebroin, M.G., Gailly, P.A., Nguyen, J.-F., Sadoun, M.J., Mainjot, A.K., Bonding to CAD-CAM composites: an interfacial fracture toughness approach. J Dent Res 97 (2018), 60–67, 10.1177/0022034517728714.
Özcan, M., Nijhuis, H., Valandro, L.F., Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging. Dent Mater J 27 (2008), 99–104, 10.4012/dmj.27.99.
Tsuchimoto, Y., Yoshida, Y., Mine, A., Nakamura, M., Nishiyama, N., Van Meerbeek, B., et al. Effect of 4-MET- and 10-MDP-based primers on resin bonding to titanium. Dent Mater J 25 (2006), 120–124, 10.4012/dmj.25.120.
Tian, T., Tsoi, J.K.-H., Matinlinna, J.P., Burrow, M.F., Aspects of bonding between resin luting cements and glass ceramic materials. Dent Mater 30 (2014), e147–e162, 10.1016/j.dental.2014.01.017.
Yano, H.T., Ikeda, H., Nagamatsu, Y., Masaki, C., Hosokawa, R., Shimizu, H., Correlation between microstructure of CAD/CAM composites and the silanization effect on adhesive bonding. J Mech Behav Biomed Mater, 101, 2020, 103441, 10.1016/j.jmbbm.2019.103441.
Willers, A.E., Gomes Araújo-Neto, V., Bosso André, C., Giannini, M., Bond durability of a silane-containing self-adhesive and conventional resin cements to CAD/CAM glass and hybrid ceramics. J Adhes Sci Technol, 2023, 1–14, 10.1080/01694243.2023.2229696.
Murakami, S., Hirano, K., Fusejima, F., Bonding durability of resin cement to lithium disilicate glass ceramics. Dent Mater, 38, 2022, e31, 10.1016/j.dental.2021.12.081.
Chen, C., Chen, Y., Lu, Z., Qian, M., Xie, H., Tay, F.R., The effects of water on degradation of the zirconia-resin bond. J Dent 64 (2017), 23–29, 10.1016/j.jdent.2017.04.004.
Soto-Montero, J., Missiato, A.V., Dias, C.T.D.S., Giannini, M., Effect of airborne particle abrasion and primer application on the surface wettability and bond strength of resin cements to translucent zirconia. J Adhes Sci Technol 37 (2023), 1458–1470, 10.1080/01694243.2022.2079326.
Bagegni, A., Borchers, J., Beisel, S., Patzelt, S.B.M., Vach, K., Kohal, R., Bonding strength of various luting agents between zirconium dioxide crowns and titanium bonding bases after long-term artificial chewing. Materials, 16, 2023, 7314, 10.3390/ma16237314.
Farahani, M., Wallace, W.E., Antonucci, J.M., Guttman, C.M., Analysis by mass spectrometry of the hydrolysis/condensation reaction of a trialkoxysilane in various dental monomer solutions. J Appl Polym Sci 99 (2006), 1842–1847, 10.1002/app.22190.
Koko, M., Takagaki, T., Abdou, A., Inokoshi, M., Ikeda, M., Wada, T., et al. Effects of the ratio of silane to 10-methacryloyloxydecyl dihydrogenphosphate (MDP) in primer on bonding performance of silica-based and zirconia ceramics. J Mech Behav Biomed Mater, 112, 2020, 104026, 10.1016/j.jmbbm.2020.104026.
Hung, S.H., Hung, K.-S., Eick, J.D., Chappell, R.P., Marginal fit of porcelain-fused-to-metal and two types of ceramic crown. J Prosthet Dent 63 (1990), 26–31, 10.1016/0022-3913(90)90260-J.
Moraes, R., Boscato, N., Jardim, P., Schneider, L., Dual and self-curing potential of self-adhesive resin cements as thin films. Oper Dent 36 (2011), 635–642, 10.2341/10-367-L.